Coating Quantity

PACKAGE SIZE / QUANTITY Coating Coverage
Resin Quantity Hardener quantity Mixed Quantity Saturation coat porous surfaces Buildup coats non-porous surfaces
105-A
1 qt (.94L)
2.40 lb
205-A or 206-A
.43 pt (.20 L)
.47 lb
1.2 qt (1.15 L)
2.87 lb
90-105 ft²
(8.5-10m²)
120 - 135 ft²
(11-12.5m²)
207-A or 209-A
.66 pt (.31 L)
.70lb
1.3 qt (1.26 L)
3.1 lb
90-105 ft²
(9-10 m²)
120-135 ft²
(11-13 m²)
105-B
.98 gal (3.74 L)
9.50 lb
205-B or 206-B
.86 qt (.81 L)
1.86 lb
1.2 gal (4.55 L)
11.36 lb
350-405 ft²
(32-37 m²)
462 - 520 ft²
(43-48 m²)
207-B or 209-B
1.32 qt (1.24 L)
2.75 lb
1.3 gal (4.98 L)
12.25 lb
370-430 ft²
(35-40 m²)
490-550 ft²
(45-50 m²)
105-C
4.35 gal (16.46 L)
41.82 lb
205-C or 206-C
.94 gal (3.58 L)
8.20 lb
5.29 gal (20 L)
50.02 lb
1530-1785 ft²
(142-165 m²)
2040-2300 ft²
(190-213 m²)
207-C or 209-C
1.45 gal (5.49 L)
12.0 lb
5.8 gal (21.9 L)
53.82 lb
1675-1955 ft²
(155-180 m²)
2235-2520 ft²
(207-233 m²)