Approximate mixed epoxy required to produce a catsup, mayonnaise or peanut butter consistency for the various sized filler products at 72°F. Mixtures may require more filler/less epoxy at higher temperatures.

Filler Package size Quantity of mixed epoxy required for
catsup consistency mayonnaise consistency peanut butter consistency
403-9
403-28
403-B
6.0 oz
20.0 oz
20.o lb
3.8 qt
3.2 gal
48.0 gal
2.5 qt
2.0 gal
32.0 gal
1.0 qt
.9 gal
15.3 gal
404-15
404-45
404-B
15.2 oz
43.0 oz
30.0 lb
1.2 qt
3.6 qt
9.4 gal
.9 qt
2.8 qt
7.4 gal
.7 qt
2.0 qt
5.3 gal
405 8.0 oz .9 qt .7 qt .6 qt
406-2
406-7
406-B
1.7 oz
5.5 oz
10.0 lb
1.3 qt
1.1 gal
27.0 gal
.9 qt
3.0 at
16.0 gal
.5 qt
1.7 qt
6.0 gal
407-5
407-15
407-B
4.0 oz
12.0 oz
14.0 lb
.5 qt
1.7 qt
6.0 gal
.4 qt
1.3 qt
4.8 gal
.3 qt
1.0 qt
3.7 gal
410-2
410-7
410-B
2.0 oz
5.0 oz
4.0 lb
1.2 qt
3.0 qt
8.9 gal
.9 qt
2.4 qt
7.2 gal
.7 qt
1.8 qt
5.6 gal