| HARDENER | USES Resin/Hardener | HARDENER TEMPERATURE RANGE (°F) | CURE SPEEDS at room temp * | ||
|---|---|---|---|---|---|
![]() |
POT LIFE 100g cupful |
WORKING TIME thin film |
CURE TO SOLID thin film |
||
| 205 Fast Hardener | General Bonding, fabric application and barrier coating | ![]() |
9-12 min |
60-70 min |
6-8 hours |
| 206 Slow Hardener | General bonding, fabric application and barrier coating | ![]() |
20-25 min |
90-110 min |
10-15 hours |
| 209 Extra Slow Hardener | General bonding, fabric application and barrier coating | ![]() |
40-50 min |
3-4 hours |
20-24 hours |
| 207 Special Clear Hardener | Clear fabric application and clear coating for a natural wood finish | ![]() |
20-26 min |
100-120 min |
10-15 hours |
*Epoxy cures faster in warmer temperatures and in thicker applications—Epoxy cures slower in cooler temperatures and in thinner application